AWS A5.8 BCuP-6
DIN EN1044 CP 105
DIN 8513 L-Ag2P
ISO 17672 CuP 279
Cu | P | Ag |
---|---|---|
92 | 6 | 2 |
Acetylene torch, induction and resistance heating
Copper-phosphorus alloy with low silver content. This alloy has good gap filling properties and it is well suited to bridge wide gaps. Suitable for gap brazing of copper and copper alloys. Approved by DVGW-worksheet GW 2 for copper pipes. Joint-brazing at working temperatures between -60 °C and +150 °C*. Do not use in sulphurous environment and on Fe- and Ni-alloys
Rods: φ1.5-5.0mm Length: 50-1000mm
Wire and Flat wire: φ0.8, 1.0, 1.2, 1.6mm
Other dimensions are available upon request
Working temperature: 740 °C
Melting range: 643- 790 °C
Specific gravity: 8.1 g/cm³
Tensile strength: 250 N/mm²
Elongation: 5 %
You might like