CuMn12Ni2
EN ISO 3677: B-Cu86MnNi-970/990
Cu | Mn | Ni |
---|---|---|
86.0 | 12.0 | 2.0 |
Working temperature: 990 °C
Melting range: 960 - 990 °C
Specific gravity: 8.4 g/cm³
Tensile strength: 390 N/mm²
Brazing
Manganese bearing copper based alloy for capillary brazing of alloyed and
unalloyed steel. Well suited for hard metal / steel joints..
Rods: φ1.5-5.0mm Max.Length: 15mm-1000mm
Wire: φ1.2,1.6mm on spools or coil wire
Other dimensions are available upon request