AWS A5.8 RBCuZn-D
DIN EN1044 CU305
DIN 8513 L-CuNi10Zn42
ISO 17672 Cu773
Cu | Ni | Si | Zn | Other |
---|---|---|---|---|
46-50 | 9-11 | 0.04-0.25 | Balance | 0.5 |
Acetylene torch, induction and resistance heating
Flux: Borax, Borax acid and agglomerant.
Nickel-bearing filler metal of high strength and good fluidity. Suitable for brazing of steel, cast iron, malleable cast iron, nickel and nickel alloys. Suitable for brazing and hardening in one production step. It is very often used in the steel furniture industry.
φ1.5-4.8mm Max.Length: 1000mm
Working temperature: 940-980 °C
Melting range: 921 - 935 °C
Specific gravity: 8.7 g/cm³
Tensile strength: 690 N/mm²
Elongation: 15-20 %
You might like